Does anyone could share their experience with AFE4500 solder ball crack impaction of PPG reading?
We have observe the below phenomenon during my failure analysis finding:
Low PPG DLP reading from the AFE4500 IC with half-cracked or non-spherical balls, the low DLP reading issue can be resolved when we reheat the AFE4500.
My Question is, does half-cracked or non-spherical balls impact the PD value?
BR,
Paul